What is the reason for the short start-up cycle of WPC floor?


Reason analysis: The formula structure is unreasonable, the stabilizer plasticizing is slow and the stabilization time is not stable enough, which directly affects the production cycle.


Solution: Properly adjust the formula, increase the amount of stabilizer, and increase the overall lubrication system.


Why do bubbles (pinholes) appear on the broken surface of WPC floor? Reason analysis: The overall reason for this situation is mainly caused by the unreasonable connection between the plasticizing time and the foaming time or the lack of the entire melt strength.


Solution: The current market stabilizers are diverse and complex, with uneven levels.


Reason analysis: uneven discharge. Solution: The opening of the die lip can be adjusted. If the flow rate is too large, the choke rod can be adjusted, and the amount of internal and external lubricants can be adjusted according to the actual situation.


At the same time, the processing modifier P-107 can be added to the plate of different thickness to increase the plasticization and dispersibility of the material during the extrusion process, and at the same time increase the toughness of the substrate and the fineness of the emptying.